WOODRESEARCH: Vol.57 No.3 2012

CONTENTS
1. EDWARD ROSZYK, PRZEMYSŁAW MANIA, WALDEMAR MOLIŃSKI: The influence of microfibril angle on creep scotch pine wood under tensile stress along the grains . . . 347
2. PETR HORÁČEK, JAN TIPPNER, KHALED T. HASSAN: Nondestructive evaluation of static bending properties of scots pine wood using stress wave technique... 359
3. RICHARD HRČKA, MARIAN BABIAK: Some non-traditional factors influencing thermal properties of wood . . . 367
4. ERGUN BAYSAL: Surface characteristics of CCA treated Scots pine after accelerated weathering . . . 375
5. MICHAL KLOIBER, JAN TIPPNER, LUDĚK PRAUS, JAROSLAV HRIVNÁK: Experimental verification of a new tool for wood mechanical resistance measurement . . . 383
6. KIRIAKI GIAGLI, ELIAS VOULGARIDIS: Investigation on the appearance of cracks in logs after felling and bucking of trees in a poplar (I-214) plantation . . . . 399
7. MILAN DEMO, DUŠAN HÚSKA, ZUZANA POLÁKOVÁ: Impact of soil-climatic and hydrological conditions southwestern Slovakia to the production indicators of fast growing willow Salix . . . 409
8. MICHAL JABLONSKÝ, MARTINA BOTKOVÁ, KATARÍNA HROBOŇOVÁ: Accelerated ageing of wood-containing papers: Formation of weak acids and deterioration of tensile strength . . . 419
9. XIAOLI GU, CHENG LIU, HENG YIN, XUEWEI MENG, KANGHUA CHENG, MING HE ZHONGZHENG LI: Study on pyrolysis of sawdust under different heating rates by using TG-FTIR analysis . . . 435
10. ZEKI CANDAN, TURGAY AKBULUT, SIQUN WANG, XINAN ZHANG, A. FARUK SISCI: Layer thickness swell characteristics of medium density fibreboard (MDF) panels affected by some production parameters . . . 441
11. NEJC THALER, MIHA HUMAR, BOŠTJAN LESAR: Performance of selected copper amine based wood preservative supplemented with wood swelling agents . . . . .453
12. PIOTR WITOMSKI, JANUSZ ZAWADZKI, ANDRZEJ RADOMSKI: Changes of the pine wood (Pinus sylvestris L.) chemical composition during white- and brown-rot decay originated from chosen fungi species . . . 463
13. IGOR DŽINČIĆ, DUŠAN SKAKIĆ: Influence of type of fit on strength and deformation of oval tenon-mortise joint . . . 469
14. JERZY MAJKA: The influence of fan speed reduction on airflow uniformity in timber stack during kiln drying . . . 479
15. ELIAS VOULGARIDIS, COSTAS PASSIALIS, MARTINO NEGRI, STERGIOS ADAMOPOULOS: Shear bond strength of black locust wood glued with three adhesive systems . . . 489
16. ERIK BARADIT, PETER NIEMZ: SHORT NOTE - Elastic constants of some native chilean wood species using ultrasound technique . . . 497


Contents

Download WR20120300 Contents


Download WR20120301 Articles


Download WR20120302 Articles


Download WR20120303 Articles


Download WR20120304 Articles


Download WR20120305 Articles


Download WR20120306 Articles


Download WR20120307 Articles


Download WR20120308 Articles


Download WR20120309 Articles


Download WR20120310 Articles


Download WR20120311 Articles


Download WR20120312 Articles


Download WR20120313 Articles


Download WR20120314 Articles


Download WR20120315 Articles


Download WR20120316 Articles


© ŠDVÚ 2009