Quality evaluation of UHF RFID antennas and passive tags on paper substrates

The effect of antenna design modification, paper substrates and relative electrical permittivity of background materials on the reflection coefficient of UHF RFID antennas was studied. Simulation software was used to modify the design and calculate the reflection coefficient of the antennas. By modifying the coupling of the dipole with the induction loop of the antennas, a reduction of the simulated reflection coefficient was achieved compared to the commercial antenna. The positive effect of antenna modification was also confirmed by measuring the reflection coefficient of antennas printed on paper by thermal transfer printing, placed on extruded polystyrene and particle board. The reflection coefficient of the modified antennas was lower when placed on extruded polystyrene, whose relative electrical permittivity was lower than particle board. After installing the memory chip to the antennas printed on paper and paperboard, the identification, reading and recording range of passive UHF RFID tags were measured after they were placed on thicker paperboard, extruded polystyrene and particle board. The positive effect of antenna modification on improving the communication quality of passive UHF RFID tags placed on background materials with a relative electrical permittivity of 2.4 to 6.7 was confirmed.

Effect of paperboard surface modifications on electrical conductivity of printed UHF RFID antennas

The effect of surface roughness and water contact angle of commercial paperboard before and after surface modification by calendering, coating and calendering and plasma treatment on the functionality of UHF RFID antennas printed with thermal transfer aluminum ribbon was evaluated. A hydrophilic surface was created by coating or plasma treatment, which improved the wettability of the paperboard surface, the spreading of the thermoplastic tie layer and the adhesion of the conductive aluminum layer. A new paper product was created with permanent surface wettability by coating, without the need for plasma treatment before printing. The plasma treatment provided time-limited wettability, needed only during printing, and made it possible to restore the original hydrophobic surface of the paperboard. In addition to the meaning of these surface modifications, the importance and need to reduce the surface roughness was confirmed, as the higher surface roughness of the paperboard limited the effect of the plasma treatment in terms of its printability and the functionality of the printed aluminum antenna. The printability of the paperboard and the functionality of the printed antennas were evaluated using electrical conductivity. The electrical conductivities of the dipole and inductor loop of the UHF RFID antennas printed on modified paperboards varied depending on the antenna design.

Effect of smoothing in calender and hot stamping machine on the properties of coated paperboards for printed electronics

The methods of coated paperboards smoothing with a hot stamping machine using a smooth metal die and a conventional calender were compared. The printing roughness required for printing electrical and electronic components was achieved by both smoothing methods. The printing roughness of the coated paperboards decreased after hot stamping by 18 to 42% and after calendering by 22 to 41% depending on the grade of coated paperboard. The stiffness of coated paperboards decreased after hot stamping by only 4 to 21%, while by up to 38 to 51% after calendering. The ratio of specific stiffness and printing roughness of coated paperboards after hot stamping ranged from 2.5 to 8.1 mN. μm-2 and after calendering from 2.0 to 6.7 mN. μm-2. The stiffness of the coated paperboards decreased less after hot stamping, and that only in the printed electronics area, while after calendering the stiffness decreased significantly more in the whole profile. It can be assumed that packaging made from coated paperboards smoothed by hot stamping will have a lower weight and thus lower costs than packaging from calendered coated paperboards.

Effect of prehydrolysis on enzymatic hydrolysis of two-stage pretreated wheat straw

The effect of water prehydrolysis conditions, which was used as the first stage of wheat straw pretreatment, on the composition of filtrates was analysed. Many of the substances that are present in the prehydrolysis filtrates are broadly used and thus they contribute to improvements in the efficiency of bioethanol production. Prehydrolysis was carried out at temperatures of 140, 160 and 180°C and times of 30, 60 and 120 min. Xylose and its oligomers were the most represented in prehydrolysis filtrates, their yields increased up to 12.1 % with increasing weight of wheat straw removed up to 28.6 %. Besides xylose and glucose, acetic acid, formic acid and the phenolic compounds were also present in the prehydrolysis filtrates. At 160 and 180°C, levulinic acid and furfural and hydroxymethylfurfural, respectively, were also present. The solid fractions of wheat straw were subjected to steam explosion under the same conditions at 200°C for 2 min. Two-stage pretreated wheat straw was subsequently enzymatically hydrolysed. The conditions of water prehydrolysis combined with steam explosion pretreatment had a significant effect on the results of enzymatic hydrolysis of wheat straw. The conversion of cellulose increased with increasing prehydrolysis temperature and time from 64.8 to 91.7 %. Similar results were observed for the conversion of xylan from 73.7 to 92.4 %. With increasing of prehydrolysis temperature and time, the amount of inhibitors in hydrolysates decreased. The recommended conditions for water prehydrolysis at two-stage pretreatment of wheat straw correspond to temperature of 160°C and time of 60 min.

Effect of steam explosion temperature on wheat straw enzymatic hydrolysis

Wheat straw is an abundant and readily available lignocellulosic material potentially suitable for the second generation bioethanol production. Steam explosion was investigated as a suitable pretreatment method. Effect of steam explosion temperature on wheat straw enzymatic hydrolysis was investigated. Optimum steam explosion temperature at around 200°C was determined based on concentration of monosaccharides in hydrolysates, conversion of cellulose and xylan and yield of monosaccharides from wheat straw. This corresponds to creating conditions resulting in sufficient damage to the lignocellulose structure which leads to higher enzyme accessibility. Lower temperature does not enable sufficient enzyme accessibility while excessively high temperature results in significant breakdown of monosaccharides and lignin and creation of inhibitors. The amount of originated inhibitors was also determined for each studied steam explosion temperature.

Enzymatic hydrolysis of extruded wheat straw with addition of sodium hydroxide and calcium hydroxide

Extrusion pretreatment of wheat straw in a single screw extruder was investigated in terms of effectiveness of enzymatic hydrolysis and the formation of fermentation inhibitors. The effect of sodium hydroxide in extrusion pretreatment was compared with calcium hydroxide. The accessibility of wheat straw structure to hydrolytic enzymes increased with NaOH and Ca(OH)2 loadings, whereby more with the addition of NaOH. With 6% w/w of NaOH loading, the conversion of polysaccharides was 76.1% and with the same Ca(OH)2 loading it was 47.3%. The conversion of polysaccharides with 12% w/w of Ca(OH)2 loading was 66.6%. Without alkali in extrusion pretreatment, the conversion of polysaccharides was only 36.7%. The polysaccharides conversion of original extruded wheat straw was about 1.5 to 3.3% higher in comparison to washed extruded wheat straw. Fermentation inhibitors such as lignin, acetic and formic acid are primarily formed in the presence of alkali during extrusion pretreatment, most of which was lignin. Alkaline extrusion is a suitable method for pretreatment of lignocellulosic biomass.

Comparison of capillary flow porometry and mercury intrusion porosimetry in determination pore size distribution of papers

Capillary flow porometry and mercury intrusion porosimetry achieved a good agreement in determining the pore size distribution in papers for the top layers of corrugated board. Differences in the papers composition as well as structure can be easily detected by changes in the measured parameters, thus allowing a better understanding their behaviour at processing and use. Water absorption is mainly dependent on the diameter of the large pore and to a lesser extent from the diameter of medium pore, surface free energy of paper and the swelling ability of recycled and bleached pulp fibres.

Improvement of oil and grease resistance of cellulosic materials

The oil and grease resistance of paper after surface sizing with aqueous dispersions composed of film forming polymers, their mixtures with fluorinated polymer or fluorinated polymer and silver nanoparticles was compared. The oil and grease resistance of paper was regulated by changing the composition and intake of aqueous dispersions and paper grade, and it was evaluated by the content of fine surface pores, contact angle, oil absorptiveness, grease resistance, oil repellency on the inclined surface and oil penetration time. The aqueous dispersions were applied on one side and on both sides of paper surface in the size press. The film forming polymer has created a physical barrier against oil and grease, while combination with the fluorinated polymer developed a physical and chemical barrier. The papers sized with aqueous dispersions containing a mixture of film forming and fluorinated polymer with the addition of silver nanoparticles, achieved high oil and grease resistance even with lower consumption of the fluorinated polymer, and also achieved an antimicrobial surface. The more porous paper has achieved the required oil and grease resistance at higher polymers intake.

Oxidative and reductive bleaching of deinked pulp

Deinked pulps for hygienic paper production were bleached with hydrogen peroxide and sodium dithionite in single and two-stage bleaching. The brightness gain of high brightness deinked pulp in the peroxide stage was 5.7% ISO and of low brightness 4.4% ISO. In sodium dithionite stage, the brightness gain of high brightness deinked pulp was 4.0% ISO and of low brightness deinked pulp 3.8% ISO. The two-stage oxidative-reductive bleaching sequence resulted in an increase of brightness by 9.7% ISO for high brightness deinked pulp and by 9.1% ISO for low brightness deinked pulp. Brightness gain in the two-stage reductive-oxidative bleaching sequence was 6.7% ISO for high brightness deinked pulp and 5.6% ISO for low brightness deinked pulp. The coordinate b* value and yellowness of deinked pulps decreased in sodium dithionite bleaching stage more than in hydrogen peroxide stage. The two-stage oxidative-reductive bleaching sequence is more preferred than reductive-oxidative sequence regardless of the fibre composition. The tensile index and the tensile energy absorption index of deinked pulps slightly decreased after single-stage and two-stage bleaching sequences, their reduction in the peroxide stage was greater than in the dithionite stage. The fibre strength and fibre length characteristics of deinked pulps decreased after bleaching, while fibre bonding ability increased. The water absorption and bulk softness increased after bleaching, the increase was higher after peroxide stage than dithionite stage.

Blending impact of hardwood pulps with softwood pulp on tissue paper properties

The influence of proportions of bleached birch, eucalyptus, beech kraft pulps as well as the bleached aspen chemi-thermomechanical pulp (BCTMP) in the mixture with bleached pine kraft pulp on tissue paper properties was compared. Increase of bleached beech kraft pulp and aspen BCTMP proportion in a mixture with bleached pine kraft pulp leads to significant rise of porosity ε as well as bulk. The water absorption after immersion increased significantly with increase of aspen BCTMP content in the mixture while other hardwood pulps in the mixture had only moderate impact. Increasing of bleached beech and eucalyptus kraft pulps content in the mixture continually increased initial water absorption. As a result of blending of bleached birch kraft pulp with bleached pine kraft pulp, bulk softness improved and the tensile index increased slightly. The increased content of bleached birch and beech kraft pulp in the mixture increased the brightness while the addition of aspen BCTMP and bleached eucalyptus kraft pulp increased of coordinate b* value. Mixed pulps with properties suitable for different types of hygienic products were selected.

Paper substrates for inkjet printing of uhf rfid antennas

Conventional papers are not suitable for printed electronics because they have a rougher surface than the plastic film commonly used for electronics printing. The paper surfaces were modified by coating and calendering processes to reduce surface roughness and electrical resistance of inkjet-printed UHF RFID antennas. The composition of coatings, the main component which included aluminum oxide pigment, had an influence on the surface roughness, the surface pore content and the electrical resistance of the inkjet-printed UHF RFID antennas on coated papers. Papers coated with a mixture containing 25% polyvinyl alcohol binder in combination with the cationic polymer PDADMAC without glyoxal crosslinker had the lowest surface roughnesses and the lowest electrical resistances of the inkjet-printed antennas. As the coating basis weight increased, the electrical resistance of the antennas increased. Reduction of the electrical resistance of the antennas was achieved after calendering coated paper. The design of the antennas had a significant effect on their electrical resistance, which increased with the length of the antenna.

Relationship between structural parameters and water absorption of bleached softwood and hardwood kraft pulps

The influence of porosity, relative bonded area and air permeability on water absorption of unbeaten and beaten bleached kraft pulps from different wood species used for tissue paper production was investigated. The water absorption was determined by four different methods such as absorption of water after immersion, initial water absorption, water absorption capacity and saturation rate with water. Linear dependences between water absorption parameters and the structural parameters of individual pulps as well as all tested pulps were obtained. The correlation coefficients obtained within individual bleached kraft pulps were from 0.95 to 1.00 and within the whole group of pulps were from 0.86 to 0.98. Relative bonded area and air permeability were found to be the most suitable parameters for predicting of initial water absorption and saturation rate with water.

Effect of addition of deinked pulp to bleached kraft pulp on tissue paper properties

The influence of addition of deinked pulps with low and high brightness to bleached eucalyptus and pine kraft pulps on functional tissue paper properties was studied. Deinked pulps with low and high brightness had some different functional properties. Deinked pulp with high brightness has higher bulk, porosity, water absorption after immersion, initial water absorption, bulk softness as well as brightness. On the contrary, the difference in relative bonded area and porosity e between deinked pulps with low and high brightness was moderate. The mixed pulps laboratory pulp sheets from bleached eucalyptus kraft pulp or bleached pine kraft pulp with addition of 20, 40 and 80% of deinked pulp with low brightness or deinked pulp with high brightness were prepared. The addition of the deinked pulp with high or low brightness to bleached kraft pulp leads to increasing of bulk, bulk softness as well as high water absorption after immersion and initial water absorption. The tensile index rapidly decreased by the addition of deinked pulps with high brightness to bleached eucalyptus and pine kraft pulps. Similarly, the addition of deinked pulp with low brightness to bleached pine kraft pulp led to rapid decreasing of tensile index. On contrary, with the addition of deinked pulp with low brightness to eucalyptus kraft pulp, the decreasing of tensile index was less pronounced. Mixed pulp from bleached eucalyptus kraft pulp with a small content of deinked pulp with low brightness with functional properties suitable for production of tissue papers was found as optimal.

Comparison of thermal transfer and inkjet printing of UHF RFID tag antennas on paper substrates

UHF RFID printed antennas on conventional and experimentally coated papers by thermal transfer and inkjet technique were not conductive due to high surface roughness. Reducing the surface roughness of paper and hence the electrical resistance of the antennas printed by thermal transfer and inkjet printing was achieved by coating and subsequent calendering process. Papers for thermal transfer and inkjet printed of aluminum and silver antennas were prepared by coating with top functional coating, whose main component was pigment – precipitated calcium carbonate with addition of polyvinyl alcohol, cationic polymer PDADMAC and glyoxal. The desired quality of inkjet-printed silver antennas was achieved by using coated paper with a polyvinyl alcohol barrier layer and a top functional hydrophilic layer. Silver nanoparticles of inkjet ink require a sintering process to obtain a conductive printed trace. The microstructure and thickness of antennas printed by thermal transfer and inkjet technique were compared. Thermal transfer printing created a more homogeneous antenna with greater sharpness of drawing compared to inkjet printing.