Authors
-
Vladimír Duchoň
Slovak University of Technology in Bratislava, Faculty of Civil Engineering, Department of Steel and Timber Structures, Bratislava, Slovak Republic
-
Tomáš Klas
Slovak University of Technology in Bratislava, Faculty of Civil Engineering, Department of Steel and Timber Structures, Bratislava, Slovak Republic
-
Orsolya Katona
Slovak University of Technology in Bratislava, Faculty of Civil Engineering, Department of Steel and Timber Structures, Bratislava, Slovak Republic
-
Ján Brodniansky
Slovak University of Technology in Bratislava, Faculty of Civil Engineering, Department of Steel and Timber Structures, Bratislava, Slovak Republic
-
Ľuboš Balcierák
Slovak University of Technology in Bratislava, Faculty of Civil Engineering, Department of Steel and Timber Structures, Bratislava, Slovak Republic
-
Jaroslav Sandanus
Slovak University of Technology in Bratislava, Faculty of Civil Engineering, Department of Steel and Timber Structures, Bratislava, Slovak Republic
-
Kristian Sógel
Slovak University of Technology in Bratislava, Faculty of Civil Engineering, Department of Steel and Timber Structures, Bratislava, Slovak Republic