Comparative Surface Roughness Evolution of 33 Japanese Hardwoods after Water and Fire-Retardant Treatments Using 3D Optical Profilometry

Authors

  • JEONBUK NATIONAL UNIVERSITY, SOUTH KOREA

  • Jeonbuk National University, Institute of Human Ecology, College of Human Ecology, Department of Housing Environmental Design and Research, Jeonju 54896, Korea

  • JEONBUK NATIONAL UNIVERSITY, KOREA

  • KYUSHU UNIVERSITY, JAPAN

  • Kyushu University, Department of Agro-Environmental Sciences, 744 Motooka, Nishi-ku, Fukuoka, 819-0395, Japan

  • JEONBUK NATIONAL UNIVERSITY, SOUTH KOREA