Evaluation of Some Mechanical Properties of Metal-Mesh Reinforced Poplar Laminated Veneer Lumber

Author

  • Bekir Cihad Bal

    Kahramanmaraş Sütçü İmam University, Türkiye

Post Views: 364
Posted in WOOD RESEARCH Volume 71, Number 3, 2026Tagged LVL, mechanical properties, poplar veneer, reinforcement

Search for a Keyword

Cite This Article

BAL, B. (2026): Evaluation of some mechanical properties of metal-mesh reinforced poplar laminated veneer lumber. In: Wood Research 71 (3), 482-489 pp., available at: doi.org/10.37763/wr.1336-4561/71.3.482489

Articles in this Release

  • Investigation of Gamma Radiation Shielding Properties of Acacia Mangium Wood…

  • Identification of Fungal Organisms Present in Elements Considered Historical Heritage

  • Analysis of the Static Equilibrium Equation of the Oval Mortise…

  • Comparative Surface Roughness Evolution of 33 Japanese Hardwoods after Water…

  • The Study on the Frequency Response Characteristics of Wood Orthotropy…

  • Bioremediation of Wood Treated with CCA-C, ACQ, and MCQ Wood…

  • Evaluation of Some Mechanical Properties of Metal-Mesh Reinforced Poplar Laminated…

  • Influence of Traditional Plaster Layer on the Combustion Performance of…

  • Variation of Growth Characteristics and Stress-Wave Velocity of the First…

  • Experimental Investigation of Load Redistribution in a Historic-Type Timber Roof…

  • THE EFFECTS OF INTERFACIAL MODIFICATIONS ON THE PROPERTIES OF BAMBOO FIBER…

  • Surface Preparation for Lamination of OSB with Phenol Formaldehyde Film…

  • Preliminary Evaluation of Copper Leaching from Commercially Available Wood Species…

  • VARIATION IN BASIC DENSITY AND TRANSVERSE SHRINKAGE AMONG SIX EUCALYPTUS…

  • Short notes. COMPARATIVE STUDY OF THE IMPACT OF THERMAL MODIFICATION…

Copyright © 2026 Wood Research – VUPC, a.s. (Pulp and Paper Research Institute)
Wood Research
Manage Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}