Effect of Freeze–Thaw Cycle on the Screw-Holding Strength of Plywood

In this study, five-layered plywood boards were produced with poplar, beech, and eucalyptus rotary peeled veneer. One control group and three experimental group test samples were prepared from the produced boards. The experimental group test samples were subjected to 2, 4, and 6 freeze–thaw cycles according to TS EN 321. The density, moisture content, and screw-holding strength of each test sample were determined. Screw-holding tests were performed according to the principles specified in TS EN 13446. In the tests, a screw was applied perpendicular to the surface of the test sample. The poplar plywood had the lowest screw holding strength, with the highest found in the beech plywood. The effects of 4 and 6 freeze–thaw cycles on the screw-holding strength were statistically significant. A strong relationship was found between the screw-holding strength and density of the plywood.

Evaluation of Some Mechanical Properties of Metal-Mesh Reinforced Poplar Laminated Veneer Lumber

This study aimed to reinforce laminated veneer lumber boards produced with poplar veneers using metal mesh. The metal mesh and poplar veneers were bonded using polyurethane adhesive. A control group (group 1) and three experimental groups were formed. The metal mesh was placed inside the two outermost adhesive layers in group 2, inside the four outermost adhesive layers in group 3, and on the bottom surface (tensile zone) of the board in group 4. The modulus of rupture, modulus of elasticity in bending, splitting strength, and adhesion strength of the produced boards were investigated. According to the data obtained, the modulus of rupture and modulus of elasticity increased in the reinforced groups. Although the reinforcement in one group reached 20%, the other groups had smaller values. Therefore, the reinforcement effect of the metal mesh on the flexural properties remained limited. The splitting strength increased significantly. Compared to the control group, the splitting strength of group 3 increased by approximately 80%. The adhesion strength decreased slightly in the reinforced groups.