Authors
-
ALBERT RUSS
PULP AND PAPER RESEARCH INSTITUTE, SLOVAK REPUBLIC
-
ANDREJ PAŽITNÝ
PULP AND PAPER RESEARCH INSTITUTE, SLOVAK REPUBLIC
-
JURAJ KRIŠTA
PULP AND PAPER RESEARCH INSTITUTE, SLOVAK REPUBLIC
-
EMMA WESZELOVSZKÁ
PULP AND PAPER RESEARCH INSTITUTE, SLOVAK REPUBLIC
-
VLADIMÍR IHNÁT
SLOVAK FOREST PRODUCTS RESEARCH INSTITUTE, SLOVAK REPUBLIC