Porosity and pore size distribution of recent and ancient buried Phoebe Zhennan wood determined by mercury intrusion porosimetry

Authors

  • Sichuan Agricultural University, China
    Key Laboratory of Wood Industry And Furniture Engineering of Sichuan Provincial Colleges And Universities, China

  • Sichuan Agricultural University, China
    Key Laboratory of Wood Industry And Furniture Engineering of Sichuan Provincial Colleges And Universities, China

  • Sichuan Agricultural University, China
    Key Laboratory of Wood Industry And Furniture Engineering of Sichuan Provincial Colleges And Universities, China

  • Sichuan Agricultural University, China
    Key Laboratory of Wood Industry And Furniture Engineering of Sichuan Provincial Colleges And Universities, China

  • Sichuan Agricultural University, China
    Key Laboratory of Wood Industry And Furniture Engineering of Sichuan Provincial Colleges And Universities, China

  • Sichuan Agricultural University, China
    Key Laboratory of Wood Industry And Furniture Engineering of Sichuan Provincial Colleges And Universities, China

  • Sichuan Agricultural University, China
    Key Laboratory of Wood Industry And Furniture Engineering of Sichuan Provincial Colleges And Universities, China